German Rochling Gray Durostone CFR767
The combination of processing cycles in high temperature environments combined with aggressive fluxes can cause degradation of standard Durostone grades.
The solution is Durostone CFR767, which is specially formulated for aggressive fluxes and high temperature process configurations.
The resin used to produce Durostone CFR767 can withstand temperatures up to 300°C. When the solder bath temperature exceeds 265°C and the bottom PCB preheat exceeds 140°C, Durostone CFR767 should be used instead of the standard grade.
Durostone CFR767 has excellent flux resistance. When fluxes containing halides or dicarboxylic acids are used in high-volume production, the lifetime of standard grade materials is reduced, so Durostone CFR767 is the ideal solution.
November 14, 2024
November 13, 2024
October 20, 2022
October 20, 2022
November 13, 2024
November 03, 2024
Envíeo por correo a este provedor
November 14, 2024
November 13, 2024
October 20, 2022
October 20, 2022
November 13, 2024
November 03, 2024
Declaración de privacidade: a súa privacidade é moi importante para nós. A nosa empresa promete non divulgar a súa información persoal a ningunha expansión con os seus permisos explícitos.
Encha máis información para que poida poñerse en contacto contigo máis rápido
Declaración de privacidade: a súa privacidade é moi importante para nós. A nosa empresa promete non divulgar a súa información persoal a ningunha expansión con os seus permisos explícitos.